Welcome Customer !

Membership

Help

Shanghai Bairuo Testing Instrument Co., Ltd
Custom manufacturer

Main Products:

mechb2b>Products

Slow strain rate stress corrosion testing machine

NegotiableUpdate on 02/01
Model
Nature of the Manufacturer
Producers
Product Category
Place of Origin

Overview

This slow strain rate (SSRT) stress corrosion cracking (SCC) testing machine is mainly used to detect and study the mechanical properties of metal materials in high temperature and high pressure pure water, supercritical water, and water environments containing trace amounts of alkaline, acidic, salt and other impurities, such as static tensile strength, creep, stress corrosion, etc. It can also be used to test the stress corrosion damage characteristics of metals in media environments with higher concentrations of NaOH, Na2CrO4, N2O4, HNO3, NH3OH, H2S, Cl - containing solutions, methanol, phosphate ester hydraulic oil, acetic acid and other media.

Product Details




:

Lin Xinsheng

:/

Fax number:

Address:market@bairoe.com info@bairoe.com



Equipment description of slow strain rate stress corrosion testing machine:

Slow strain rate(SSRT)Stress corrosion(SCC)The testing machine is mainly used to simulate the tensile, compressive, bending, creep and other tests of metal, non-metal, composite materials and their finished products under different working conditions such as temperature, pressure and environmental media, according to the requirements of use, to test the stress corrosion resistance of materials under slow rate conditions.

This testing machine is a new type of microcomputer controlled slow strain rate stress corrosion testing machine jointly developed by Shanghai Bairuo Testing Instrument Co., Ltd. and Shanghai Jiao Tong University. It uses high-precision sensors for force measurement, high-speed and ultra high resolution data acquisition cards for data acquisition, and computer load, time, deformation, displacement and other numerical and graphical display and processing. It can perform various control methods such as load, deformation, displacement, etc.

This machine is4A stretching head design that can simultaneously4Conduct stress corrosion testing on a sample under high temperature and high pressure environment.

Select products for key components of the equipment to ensure stable and reliable operation of the system.TestLiveThe experimental software has a fully Chinese interface and powerful data processing functions. The experimental conditions and results are automatically saved, and the experimental data, curves, and reports are displayed and printed. This machine is an ideal cost-effective experimental equipment for research institutes and colleges.

Functional characteristics of slow strain rate stress corrosion testing machine:

l Dynamic display: Load, displacement, deformation, time, and test curves are dynamically displayed in real-time on the screen.

l The load, displacement, deformation and other channels are fully closed-loop controlled, and there is no impact or smooth switching between them.

l 4Design a stretching head, collect force values simultaneously, and conduct stress corrosion tests simultaneously.

l Record and output experimental data and curves such as stress-strain, force time, and force displacement. And it can record and calculate the fracture life, tensile strength, strain, and elongation of the specimen.

l The test data can be stored in the event of a power outage, and the interrupted test can continue.

l support50Continuous experiments lasting for more than days.

l Peak display, the peak is displayed at the window position after the experiment is completed.

l Up to20The linear compensation function of the segment sensor can improve the accuracy level of the equipment.

l Domestic open experimental method setting, where administrators can establish experimental projects and operators can use these projects to conduct experiments, reducing operational difficulty;

l Domestic * experimental control process design, users can easily view the experimental control steps at a glance, with rich instruction types and support for dynamic setting of instruction parameters;

l The numerical rounding of the experimental data conforms toGB 8170-87(UDC511.1/2)Numerical rounding rules, supporting segmented rounding and custom rounding.

l The characteristic test data can be annotated and displayed on the curve graph.

l Support statistical calculation of experimental data (mean, standard deviation, coefficient of variation).

l Automatically obtain experimental data results and activate advanced analysis functions to verify the data.

l The test results can be stored and can be read and viewed at any time.

l The experimental data and curves can be reanalyzed, and the curves can be locally magnified at will.

l Open test report, supports custom report templates, automatically generates test reports, can be printed or previewed, and can be saved as files.

l Anti corrosion water tray to prevent liquid from flowing out and corroding equipment components.

l It has software limit protection, travel limit protection, and full-scale overload protection functions.

Technical specifications of slow strain rate stress corrosion testing machine:


Product Model

YYF-40

accuracy class

0.5level

The most powerful experimental force

40kN(10kN×4)

Test force measurement range

1%~F.S.

Accuracy of test force indication

±0.5%

Test force resolution

±500000Code, no grading throughout the process, unchanged resolution

Deformation measurement range

0~10mm

Relative error of deformation indication

±0.5%

Deformation resolution

0.001mm

Relative error of displacement indication

±0.5%

Displacement resolution

0.0000003mm

Range of displacement rate adjustment

0.0001~5mm/min

Relative error of displacement rate

±0.5%

Adjustment range of test force rate

0.05%~5%F.S./s

Relative error of test force rate

Speed <0.5%F.S./sTime: ±1%Speed ≥0.5%F.S./sTime: ±0.5%

Constant force, constant deformation, constant displacement control range

1%~F.S.

Constant force, constant deformation, and constant displacement control accuracy

Set value <1%F.S.Time: ±1%Set value ≥1%F.S.Time: ±0.5%

Loading head movement range

≥100mm

power supply

1.0kW/AC220V/50Hz

Overall dimensions of the host

780mm×500mm×2650mm

weight

about290kg