DSC 404 F3 Pegasus® It is one of the new members of the NETZSCH F3 series products. The instrument is designed based on the principle of thermal flow DSC, following the ISO 11357、ASTM E967、ASTM E 968、ASTM E 793、ASTM D 3895、ASTM D 3417、ASTM D 3418、DIN 51004、DIN 51007、DIN 53765 Waiting for relevant international standards. For the detection of thermal effects such as phase transition temperature and phase transition enthalpy, NETZSCH DSC 404 F3 Pegasus® It is a testing instrument with fast measurement, good reliability, and high cost-effectiveness. The high vacuum sealed system, multiple replaceable sensors, and furnace body ensure that the test results are true and reliable between -150 ° C and 2000 ° C. Multiple optional vacuum pumps, gas flow control systems, and sensors can be selected and adjusted according to the needs of the customer's application field to create a testing system.
DSC 404 F3 Pegasus® For high-precision material characterization, it is a solid, durable, and easy to operate instrument. The unique furnace body design ensures the uniform temperature performance of the furnace body, and the heat flow is evenly transmitted from all directions to the DSC sensor. Sensors have excellent sensitivity, extremely small time constants, good baseline stability, and repeatability. Therefore, the reliability of phase transition temperature testing and enthalpy testing is very high. Provide multiple replaceable DSC sensors, allowing DSC testing to be conducted between -150 ° C and 1650 ° C, and DTA sensors to be tested up to 2000 ° C.
The instrument has a high vacuum sealed system design, a metal encapsulated MFC system, a stepper motor that can assemble one to two furnace bodies, an automatic sampling system that can accommodate up to 20 samples, and a large number of optional crucible types. Therefore, this instrument can test almost all samples and has a wide range of applications. For various future applications, DSC 404 F3 Pegasus® Provides a large number of upgrade possibilities.
| Furnace body type | temperature range | cooling method |
| Silver furnace | -120 . .. 675℃ | 液氮冷却 |
| Copper furnace | -150 . .. 500℃ | 液氮冷却 |
| stainless steel furnace | -150 . .. 1000℃ | 液氮冷却 |
| Platinum furnace | RT . .. 1500℃ | Forced air cooling |
| Silicon carbide furnace | RT . .. 1600℃ | Forced air cooling |
| Rhodium furnace | RT . .. 1650℃ | Forced air |
| graphite furnace | RT . .. 2000℃ | water cooling |